Figure 11





Magnetization curves for 2-, 12- and 25-repeat (Fe40Å/Si14Å) multilayers grown during the same deposition run at nominal RT on glass substrates. The 2-repeat multilayer (really an Fe/Si/Fe trilayer) shows no signs of AF coupling. The 12-repeat multilayer appears to have a smaller coupling than the 25-repeat one.


alchaiken@gmail.com (Alison Chaiken)
Wed Oct 11 01:35:04 PDT 1995