Figure 3



Figure 3: Co-thickness dependence of the anisotropic magnetoresistance (AMR) and spin-valve magnetoresistance for a series of Fe-Cu-Co-Cu sandwiches. These samples were deposited on glass at 165 °C, and had the structure Fe56Å/Cu50Å/Co(tCo)/Cu30Å.